Surface passivation of GaAs nanowires by the atomic layer deposition of AlN

Tutkimustuotos: Lehtiartikkeli

Tutkijat

Organisaatiot

  • RAS - Ioffe Physico Technical Institute
  • St. Petersburg Academic University
  • Russian Academy of Sciences
  • St. Petersburg National Research University of Information Technologies, Mechanics and Optics (ITMO)
  • St. Petersburg State Polytechnical University

Kuvaus

It is shown that the atomic layer deposition of thin AlN layers can be used to passivate the surface states of GaAs nanowires synthesized by molecular-beam epitaxy. Studies of the optical properties of samples by low-temperature photoluminescence measurements shows that the photoluminescence-signal intensity can be increased by a factor of up to five by passivating the nanowires with a 25--thick AlN layer.