Abstrakti
High levels of clinker substitution by supplementary cementitious materials, such as slag, are necessary to decrease the CO2 emissions of concrete manufacturing. However, this leads to low early concrete strength, delaying construction schedules. In cold regions, heating is an essential part of accelerating the early hydration, thus, the strength of concrete. Therefore, this study analysed the effect of thermal activation of the concrete with 45% and 70% slag in the binder using internal electrical cable heating utilised in construction by evaluating compressive strength and heat development. In addition, non-destructive test methods, such as rebound hammer and ultrasound pulse velocity meter, were introduced to widen their application in estimating early strength development using the SonReb approach. The heating with the power of 20 W and 30 W during the first 10–15 h (11.1–16.7 kWh/m3) effectively improved the early strength of concrete with 45% and 70% slag up to 14% and 60%, respectively during the first 24 h without any strength losses at the later ages. However, considering the initially low strength values (2.5–10 MPa) of concrete with 70% slag, the heat curing resulted in about a 1 – 4 MPa increase, with a maximum rise of 7 MPa, requiring additional strategies for slag activation, for example, alkali activation, to fulfil construction requirements.
| Alkuperäiskieli | Englanti |
|---|---|
| Artikkeli | 140170 |
| Sivumäärä | 13 |
| Julkaisu | Construction and Building Materials |
| Vuosikerta | 465 |
| DOI - pysyväislinkit | |
| Tila | Julkaistu - 28 helmik. 2025 |
| OKM-julkaisutyyppi | A1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä |
Rahoitus
The work is part of LOIKKA-project which was a Finnish development project on low carbon concretes. LOIKKA-project was financed by Business Finland, Finnish cement and concrete companies as well as Concrete Industry (Betoniteollisuus ry), Finnish Transport Infrastructure Agency (Väylävirasto) and Building Construction Industry (Talonrakennusteollisuus ry).
YK:n kestävän kehityksen tavoitteet
Tämä tuotos edistää seuraavia kestävän kehityksen tavoitteita:
-
SDG 9 – Teollisuus, innovaatiot ja infrastruktuuri
-
SDG 13 – Ilmastotoimet
Sormenjälki
Sukella tutkimusaiheisiin 'Non-destructive evaluation of early strength of concrete with slag thermally activated using electrical cable'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.Projektit
- 1 Päättynyt
-
LOIKKA: Betonin CO2-päästöjen puolittaminen
Punkki, J. (Vastuullinen johtaja), Gebre, T. (Projektin jäsen), Saranya, R. (Projektin jäsen), Illarionova, E. (Projektin jäsen), Al-Neshawy, F. (Projektin jäsen), Rantala, A. (Projektin jäsen), Repo, V. (Projektin jäsen), Iqbal, A. (Projektin jäsen), Antonova, A. (Projektin jäsen), Orfanoudaki, I. (Projektin jäsen), Piironen, J. (Projektin jäsen), Alapieti, T. (Projektin jäsen) & Vähälä, I. (Projektin jäsen)
EU The Recovery and Resilience Facility (RRF)
01/03/2022 → 28/02/2024
Projekti: BF Co-Innovation
Siteeraa tätä
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver