Low temperature and high quality atomic layer deposition HfO2 coatings

Alexander Pyymaki Perros, Perttu Sippola, Elisa Arduca, Leena Sisko Johansson, Harri Lipsanen

Tutkimustuotos: Artikkeli kirjassa/konferenssijulkaisussaConference contributionScientificvertaisarvioitu

2 Sitaatiot (Scopus)

Abstrakti

Low temperature high quality thermal atomic layer deposition (ALD) HfO2 process has been developed and characterized using different oxidant sources - water, water-ozone, and ozone. Despite a low deposition temperature of 170 °C, the coatings are shown to be exhibit high optical quality, good barrier properties, environmentally stable, low impurity concentration, and other desirable material properties. The water-based process was shown to produce the highest quality coatings in terms of density, purity and stoichiometry. Using various complimentary characterization techniques on hafnia coatings deposited atop silicon, including X-ray reflectivity (XRR); ultraviolet-visible reflectometry; time-of-flight secondary ion mass spectroscopy (TOF-SIMS); and X-ray photoelectron spectroscopy (XPS) measurements, the coatings are shown to be of high quality. The developed ALD hafnia processes have exceptionally good control over layer thickness with uniformed coatings reproducibly demonstrated on 150 mm silicon wafers. Due to the exceptionally low extinction coefficient, ALD hafnia coatings of varying thickness were measured atop silicon to study the coatings anti-reflectivity behavior in the mid-ultraviolet region. The anti-reflectance performance of these single-layer coatings compares to or exceeds the performance of other reported single layer coatings. Importantly, unlike other coating technologies these ALD coatings are guaranteed to be continuous, pinhole-free and dense despite being thin (< 15nm).

AlkuperäiskieliEnglanti
Otsikko2017 IMAPS Nordic Conference on Microelectronics Packaging, NordPac 2017
KustantajaIEEE
Sivut182-185
Sivumäärä4
ISBN (elektroninen)9781538630556
DOI - pysyväislinkit
TilaJulkaistu - 26 heinäkuuta 2017
OKM-julkaisutyyppiA4 Artikkeli konferenssijulkaisuussa
TapahtumaInternational Microelectronics and Packaging Society Nordic Annual Conference - Göteborg, Ruotsi
Kesto: 18 kesäkuuta 201720 kesäkuuta 2017

Conference

ConferenceInternational Microelectronics and Packaging Society Nordic Annual Conference
LyhennettäIMAPS
MaaRuotsi
KaupunkiGöteborg
Ajanjakso18/06/201720/06/2017

Sormenjälki

Sukella tutkimusaiheisiin 'Low temperature and high quality atomic layer deposition HfO<sub>2</sub> coatings'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.

Siteeraa tätä