This article outlines an alternative flowsheet for the purification of a multi-metal industrial sidestream (16.3 g/l Ni, 0.7 g/l Co, 0.6 g/l Ca and 1.6 g/l Mg) to allow high-purity nickel recovery. The methodology comprises an initial evaporation step to achieve Ca removal followed by impurity (Ca, Mg) and valuable (Co, Ni) element separation via two-step solvent extraction with organophosphorus extractants. Results indicate that > 80% of Ca is selectively removed as CaSO4 center dot 2H(2)O by evaporation with a concentration degree > 6. In the following treatment, 90% of residual Ca (0.6 g/l) can be selectively extracted with Na-D(2)EHPA. The subsequent solvent extraction step with Na-Cyanex 272 separates Co (> 99%) and Mg (> 95%). The resultant nickel sulfate solution (61.7 g/l Ni, 0.3 g/l Mg and Co 0.007 g/l) of > 99.5% purity can be directly integrated into state-of-the-art nickel recovery processes.

Yksityiskohdat

AlkuperäiskieliEnglanti
Sivumäärä8
JulkaisuJOM
TilaJulkaistu - 4 joulukuuta 2019
OKM-julkaisutyyppiA1 Julkaistu artikkeli, soviteltu

Lataa tilasto

Ei tietoja saatavilla

ID: 39538899