Film Conformality and Extracted Recombination Probabilities of O Atoms during Plasma-Assisted Atomic Layer Deposition of SiO2, TiO2, Al2O3, and HfO2

Tutkimustuotos: Lehtiartikkeli

Standard

Film Conformality and Extracted Recombination Probabilities of O Atoms during Plasma-Assisted Atomic Layer Deposition of SiO2, TiO2, Al2O3, and HfO2. / Arts, Karsten; Utriainen, Mikko; Puurunen, Riikka L.; Kessels, Wilhelmus M.M.; Knoops, Harm C.M.

julkaisussa: Journal of Physical Chemistry C, Vuosikerta 123, Nro 44, 07.11.2019, s. 27030-27035.

Tutkimustuotos: Lehtiartikkeli

Harvard

APA

Vancouver

Author

Arts, Karsten ; Utriainen, Mikko ; Puurunen, Riikka L. ; Kessels, Wilhelmus M.M. ; Knoops, Harm C.M. / Film Conformality and Extracted Recombination Probabilities of O Atoms during Plasma-Assisted Atomic Layer Deposition of SiO2, TiO2, Al2O3, and HfO2. Julkaisussa: Journal of Physical Chemistry C. 2019 ; Vuosikerta 123, Nro 44. Sivut 27030-27035.

Bibtex - Lataa

@article{8589f717734d43fb892cbdd22f10af7f,
title = "Film Conformality and Extracted Recombination Probabilities of O Atoms during Plasma-Assisted Atomic Layer Deposition of SiO2, TiO2, Al2O3, and HfO2",
abstract = "Surface recombination of plasma radicals is generally considered to limit film conformality during plasma-assisted atomic layer deposition (ALD). Here, we experimentally studied film penetration into high-aspect-ratio structures and demonstrated that it can give direct information on the recombination probability r of plasma radicals on the growth surface. This is shown for recombination of oxygen (O) atoms on SiO2, TiO2, Al2O3, and HfO2 where a strong material dependence has been observed. Using extended plasma exposures, films of SiO2 and TiO2 penetrated extremely deep up to an aspect ratio (AR) of {\^a}900, and similar surface recombination probabilities of r = (6 ± 2) × 10-5 and (7 ± 4) × 10-5 were determined for these processes. Growth of Al2O3 and HfO2 was conformal up to depths corresponding to ARs of {\^a}80 and {\^a}40, with r estimated at (1-10) × 10-3 and (0.1-10) × 10-2, respectively. Such quantitative insight into surface recombination, as provided by our method, is essential for modeling radical-surface interaction and understanding for which materials and conditions conformal film growth is feasible by plasma-assisted ALD.",
author = "Karsten Arts and Mikko Utriainen and Puurunen, {Riikka L.} and Kessels, {Wilhelmus M.M.} and Knoops, {Harm C.M.}",
year = "2019",
month = "11",
day = "7",
doi = "10.1021/acs.jpcc.9b08176",
language = "English",
volume = "123",
pages = "27030--27035",
journal = "Journal of Physical Chemistry C",
issn = "1932-7447",
publisher = "AMERICAN CHEMICAL SOCIETY",
number = "44",

}

RIS - Lataa

TY - JOUR

T1 - Film Conformality and Extracted Recombination Probabilities of O Atoms during Plasma-Assisted Atomic Layer Deposition of SiO2, TiO2, Al2O3, and HfO2

AU - Arts, Karsten

AU - Utriainen, Mikko

AU - Puurunen, Riikka L.

AU - Kessels, Wilhelmus M.M.

AU - Knoops, Harm C.M.

PY - 2019/11/7

Y1 - 2019/11/7

N2 - Surface recombination of plasma radicals is generally considered to limit film conformality during plasma-assisted atomic layer deposition (ALD). Here, we experimentally studied film penetration into high-aspect-ratio structures and demonstrated that it can give direct information on the recombination probability r of plasma radicals on the growth surface. This is shown for recombination of oxygen (O) atoms on SiO2, TiO2, Al2O3, and HfO2 where a strong material dependence has been observed. Using extended plasma exposures, films of SiO2 and TiO2 penetrated extremely deep up to an aspect ratio (AR) of â900, and similar surface recombination probabilities of r = (6 ± 2) × 10-5 and (7 ± 4) × 10-5 were determined for these processes. Growth of Al2O3 and HfO2 was conformal up to depths corresponding to ARs of â80 and â40, with r estimated at (1-10) × 10-3 and (0.1-10) × 10-2, respectively. Such quantitative insight into surface recombination, as provided by our method, is essential for modeling radical-surface interaction and understanding for which materials and conditions conformal film growth is feasible by plasma-assisted ALD.

AB - Surface recombination of plasma radicals is generally considered to limit film conformality during plasma-assisted atomic layer deposition (ALD). Here, we experimentally studied film penetration into high-aspect-ratio structures and demonstrated that it can give direct information on the recombination probability r of plasma radicals on the growth surface. This is shown for recombination of oxygen (O) atoms on SiO2, TiO2, Al2O3, and HfO2 where a strong material dependence has been observed. Using extended plasma exposures, films of SiO2 and TiO2 penetrated extremely deep up to an aspect ratio (AR) of â900, and similar surface recombination probabilities of r = (6 ± 2) × 10-5 and (7 ± 4) × 10-5 were determined for these processes. Growth of Al2O3 and HfO2 was conformal up to depths corresponding to ARs of â80 and â40, with r estimated at (1-10) × 10-3 and (0.1-10) × 10-2, respectively. Such quantitative insight into surface recombination, as provided by our method, is essential for modeling radical-surface interaction and understanding for which materials and conditions conformal film growth is feasible by plasma-assisted ALD.

UR - http://www.scopus.com/inward/record.url?scp=85074789607&partnerID=8YFLogxK

U2 - 10.1021/acs.jpcc.9b08176

DO - 10.1021/acs.jpcc.9b08176

M3 - Article

VL - 123

SP - 27030

EP - 27035

JO - Journal of Physical Chemistry C

JF - Journal of Physical Chemistry C

SN - 1932-7447

IS - 44

ER -