Efficient surface passivation of black silicon using spatial atomic layer deposition

Tutkimustuotos: Artikkeli kirjassa/konferenssijulkaisussavertaisarvioitu

Tutkijat

Organisaatiot

  • Beneq Oy

Kuvaus

Nanostructured silicon surface (black silicon, b-Si) has a great potential in photovoltaic applications, but the large surface area requires efficient passivation. It is well known that b-Si can be efficiently passivated using conformal Atomic Layer Deposited (ALD) Al2O3, but ALD suffers from a low deposition rate. Spatial ALD (SALD) could be a solution as it provides a high deposition rate combined with conformal coating. Here we compare the passivation of b-Si realized with prototype SALD tool Beneq SCS 1000 and temporal ALD. Additionally, we study the effect of post-annealing conditions on the passivation of SALD coated samples. The experiments show that SALD passivates b-Si surfaces well as charge carrier lifetimes up to 1.25 ms are obtained, which corresponds to a surface recombination velocity Seff,max of 10 cm/s. These were comparable with the results obtained with temporal ALD on the same wafers (0.94 ms, Seff,max 14 cm/s). This study thus demonstrates high-quality passivation of b-Si with industrially viable deposition rates.

Yksityiskohdat

AlkuperäiskieliEnglanti
Otsikko7th International Conference on Silicon Photovoltaics, SiliconPV 2017
TilaJulkaistu - 21 syyskuuta 2017
OKM-julkaisutyyppiA4 Artikkeli konferenssijulkaisuussa
TapahtumaInternational Conference on Crystalline Silicon Photovoltaics - Freiburg, Germany, Freiburg, Saksa
Kesto: 3 huhtikuuta 20175 huhtikuuta 2017
Konferenssinumero: 7
http://siliconpv.com/home.html

Julkaisusarja

NimiEnergy Procedia
KustantajaElsevier
Vuosikerta124
ISSN (elektroninen)1876-6102

Conference

ConferenceInternational Conference on Crystalline Silicon Photovoltaics
LyhennettäSiliconPV 2017
MaaSaksa
KaupunkiFreiburg
Ajanjakso03/04/201705/04/2017