Abstrakti
Ni-rich layered oxides LiNi1-x-yMnxCoyO2 (NMC811, x = 0.1 and y = 0.1) are considered promising cathode materials in lithium-ion batteries (LiBs) due to their high energy density. However, those suffer a severe capacity loss upon cycling at high delithiated states. The loss of performance over time can be retarded by Zr doping. Herein, a small amount of Zr is added to NMC811 material via two alternative pathways: during the formation of the transition metal (TM) hydroxide precursor at the co-precipitation step (0.1%-Zr-cp) and during the lithiation at the solid-state synthesis step (0.1%-Zr-ss). In this work, the crystallographic Zr uptake in both 0.1%-Zr-ss and 0.1%-Zr-cp is determined and quantified through synchrotron X-ray diffraction and X-ray absorption spectroscopy. We prove that the inclusion of Zr in the TM site for 0.1%-Zr-cp leads to an improvement of both specific capacity (156 vs 149 mAh/g) and capacity retention (85 vs 82%) upon 100 cycles compared to 0.1%-Zr-ss where the Zr does not diffuse into the active material and forms only an extra phase separated from the NMC811 particles.
Alkuperäiskieli | Englanti |
---|---|
Sivut | 28683-28693 |
Sivumäärä | 11 |
Julkaisu | ACS Applied Materials and Interfaces |
Vuosikerta | 16 |
Numero | 22 |
Varhainen verkossa julkaisun päivämäärä | 20 toukok. 2024 |
DOI - pysyväislinkit | |
Tila | Julkaistu - 5 kesäk. 2024 |
OKM-julkaisutyyppi | A1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä |
Sormenjälki
Sukella tutkimusaiheisiin 'Comprehensive Study of Zr-Doped Ni-Rich Cathode Materials Upon Lithiation and Co-Precipitation Synthesis Steps'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.Laitteet
-
Raaka-aineiden tutkimusinfrastruktuuri
Karppinen, M. (Manager)
Kemian tekniikan korkeakouluLaitteistot/tilat: Facility