Skip to main navigation Skip to search Skip to main content

Yield shear stress dependence on nanoindentation strain rate in bulk GaN crystal

  • Masaki Fujikane
  • , Toshiya Yokogawa
  • , Shijo Nagao
  • , Roman Nowak
  • Panasonic Corporation
  • Norwegian University of Science and Technology

Research output: Contribution to journalArticleScientificpeer-review

28 Citations (Scopus)
Original languageEnglish
Pages (from-to)429-431
Number of pages3
JournalPhysica Status Solidi. C: Current Topics in Solid State Physics
Volume8
Issue number2
DOIs
Publication statusPublished - 2011
MoE publication typeA1 Journal article-refereed