Synthesis of a Thin-Layered Ionic Conductor, CeO2-Y2O3, by Atomic Layer Deposition in View of Solid Oxide Fuel Cell Applications

Research output: Contribution to journalArticleScientificpeer-review

Researchers

  • Elise Ballee
  • Armelle Ringuede
  • Michel Cassir
  • Matti Putkonen
  • Lauri Niinisto

Research units

Details

Original languageEnglish
Pages (from-to)4614-4619
JournalChemistry of Materials
Volume21
Issue number19
Publication statusPublished - 2009
MoE publication typeA1 Journal article-refereed