Structure and Properties of an F75 Co-Cr-Mo Superalloy Produced by Fluidized-bed Nitriding of Gas-atomized Powders, HIP-onsolidation, and Heat-treatment

W. Karlsen

    Research output: Chapter in Book/Report/Conference proceedingConference contributionScientificpeer-review

    2 Citations (Scopus)
    Original languageEnglish
    Title of host publicationSecond International Conference on Processing of Materials for Properties, San Francisco, California, November 5-8, 2000
    Pages483-488
    Publication statusPublished - 2000
    MoE publication typeA4 Article in a conference publication