Stress corrosion cracking of carbon steel in ethanolgasoline blends

Research output: Contribution to journalArticleScientificpeer-review

Researchers

Research units

  • Neste Jacobs Oy

Details

Original languageEnglish
Pages (from-to)605-612
Number of pages8
JournalMATERIALS AND CORROSION-WERKSTOFFE UND KORROSION
Volume65
Issue number6
Publication statusPublished - 2014
MoE publication typeA1 Journal article-refereed

    Research areas

  • carbon steel, ethanol–gasoline blend, intergranular, stress corrosion cracking

ID: 899652