Rare earth scandate thin films by atomic layer deposition: effect of the rare earth cation size

Pia Myllymaki, Martin Roeckerath, Joao Marcelo J. Lopes, Jurgen Schubert, Kenichiro Mizohata, Matti Putkonen, Lauri Niinisto

    Research output: Contribution to journalArticleScientificpeer-review

    21 Citations (Scopus)
    Original languageEnglish
    Pages (from-to)4207-4212
    JournalJournal of Materials Chemistry
    Volume20
    Issue number20
    DOIs
    Publication statusPublished - 2010