@inproceedings{13f90cc62c3b49c19245591b21b68098,
title = "Prediction of Stress Corrosion Cracing Susceptibility of Austenitic Stainless Steels in 50 \% CaCl2 Solution",
keywords = "corrosion, cracing, stainless steel, corrosion, cracing, stainless steel, corrosion, cracing, stainless steel",
author = "H. Leinonen and H. H{\"a}nninen",
year = "1996",
language = "English",
pages = "s. IV P 13--1 -- 13--5",
booktitle = "International Conference on Corrosion - Deformation Interactions (CDI) Eurocorr-96, Session IV, Nice, France, September 24-26, 1996",
}