Precision of nanoindentation protocols for measurement of viscoelasticity in cortical and trabecular bone

Hanna Isaksson, Shijo Nagao, Marta Malkiewicz, Petro Julkunen, Roman Nowak, Jukka S. Jurvelin

Research output: Contribution to journalArticleScientificpeer-review

63 Citations (Scopus)
Original languageEnglish
Pages (from-to)2410-2417
Number of pages8
JournalJournal of Biomechanics
Volume43
Issue number12
DOIs
Publication statusPublished - 2010
MoE publication typeA1 Journal article-refereed

Cite this