Nickel P/M superalloys with isotropic carbide reinforcement in situ

Mikhail Gasik, A. Popov

    Research output: Contribution to journalArticleScientificpeer-review

    2 Citations (Scopus)
    Original languageEnglish
    Pages (from-to)49-55
    JournalScripta Metallurgica et Materialia
    Volume32
    Issue number1
    Publication statusPublished - 1995
    MoE publication typeA1 Journal article-refereed

    Keywords

    • carbide
    • composites
    • powder metallurgy
    • superalloys