Nanoindentation and space-resolved thermal analysis of lignin-based nanofibers and films

Mariko Ago, Joseph E. Jakes, Joao V. W. Silveira, Orlando J. Rojas

Research output: Contribution to journalMeeting AbstractScientificpeer-review

Original languageEnglish
Number of pages1
JournalAbstracts of Papers of the American Chemical Society
Volume247
Publication statusPublished - 16 Mar 2014
MoE publication typeNot Eligible
EventAmerican Chemical Society National Meeting & Exposition - Dallas, United States
Duration: 16 Mar 201420 Mar 2014
Conference number: 247

Cite this