Mechanical properties characterization of c-plane (0001) and m-plane (10-10) GaN by nanoindentation examination

Research output: Contribution to journalArticleScientificpeer-review

Researchers

  • Masaki Fujikane
  • Akira Inoue
  • Toshiya Yokogawa
  • Shijo Nagao
  • Roman Nowak

Research units

  • Panasonic Corporation

Details

Original languageEnglish
Pages (from-to)1798-1800
Number of pages3
JournalPHYSICA STATUS SOLIDI C: CURRENT TOPICS IN SOLID STATE PHYSICS
Volume7
Issue number7-8
Publication statusPublished - 2010
MoE publication typeA1 Journal article-refereed

    Research areas

  • dislocations, GaN, nanoscale deformation, VPE, Young's modulus