Inorganic Hollow Nanotube Aerogels by Atomic Layer Deposition onto Native Nanocellulose Templates

Research output: Contribution to journalArticleScientificpeer-review

219 Citations (Scopus)
Original languageEnglish
Pages (from-to)1967-1974
Number of pages8
JournalACS Nano
Volume5
Issue number3
DOIs
Publication statusPublished - 2011
MoE publication typeA1 Journal article-refereed