Extensive Series of Hexagonal and Orthorhombic RMnO3 (R = Y, La, Sm, Tb, Yb, Lu) Thin Films by Atomic Layer Deposition
Research output: Contribution to journal › Article › Scientific › peer-review
Researchers
Research units
Details
Original language | English |
---|---|
Pages (from-to) | 1835-1840 |
Journal | Chemistry of Materials |
Volume | 23 |
Issue number | 7 |
Publication status | Published - 2011 |
MoE publication type | A1 Journal article-refereed |
ID: 917138