Erbium-doped waveguides fabricated with atomic layer deposition

K. Solehmainen, P. Heimala, M. Kapulainen

    Research output: Working paperProfessional

    Original languageEnglish
    Pages132
    Publication statusPublished - 2003
    MoE publication typeD4 Published development or research report or study

    Publication series

    NameNorthern Optics 2003 (NO'03). Espoo, FI, 16-18 June 2003

    Keywords

    • anions
    • Er-doped fiber
    • Fabry-Perot filter
    • industrial processes
    • integrated optics
    • on-line capillary electrophoresis
    • optical amplifiers
    • optical communications
    • pulp waters
    • ring network
    • silicon on insulator
    • WDM