Electrochemiluminescence of Tb(III) chelates at optically transparent tunnel emission electrodes fabricated by atomic layer deposition

Research output: Contribution to journalArticle

Researchers

  • Markus Håkansson
  • Mika Helin
  • Matti Putkonen
  • Qinghong Jiang
  • Mia Kotiranta
  • Johanna Suomi
  • Antti J. Niskanen
  • Timo Ala-Kleme
  • Sakari Kulmala

Research units

Details

Original languageEnglish
Pages (from-to)135-139
JournalAnalytica Chimica Acta
Volume541
Issue number1-2
Publication statusPublished - 2005
MoE publication typeA1 Journal article-refereed

    Research areas

  • Atomic layer deposition, Bioaffinity assays, Electrogenerated chemiluminescence, Hot electrons, Tb(III), Tunnel emission electrodes

ID: 2421458