Effect of pearlite on stress corrosion cracking of carbon steel in fuel-grade ethanol

Janne Torkkeli*, Tapio Saukkonen, Hannu Hänninen

*Corresponding author for this work

Research output: Contribution to journalArticleScientificpeer-review