Effect of Electrochemical Potential on Stress Corrosion Cracking Susceptibility of EN 1.4301 (AISI 304) Austenitic Stainless Steels in Simulated Hot Black Liquor

Research output: Contribution to journalArticle

Researchers

  • Pekka Pohjanne
  • Mikko Vepsäläinen
  • Timo Saario
  • Konsta Sipilä
  • Jyrki Romu

  • Tapio Saukkonen
  • Hannu Hänninen

  • Mikko Heikkilä
  • Juha Koskiniemi
  • Carl-Gustav Berg
  • Martti Pulliainen
  • Isto Virtanen
  • Thomas Ohligschläger

Research units

  • VTT Technical Research Centre of Finland
  • CSIRO
  • University of Helsinki
  • Andritz Oy
  • Savcor Forest Oy
  • Outokumpu Stainless Oy

Details

Original languageEnglish
Pages (from-to)887-894
Number of pages8
JournalCorrosion
Volume71
Issue number7
Publication statusPublished - Jul 2015
MoE publication typeA1 Journal article-refereed

    Research areas

  • alkaline solution, austenitic stainless steel, selective dissolution, sodium hydroxide, sodium sulfide, stress corrosion cracking

ID: 2013090