Atomic layer deposition of magnetic thin films : Basic processes, engineering efforts, and road forward

Topias Jussila, Anish Philip, Tripurari Tripathi, Kornelius Nielsch, Maarit Karppinen*

*Corresponding author for this work

Research output: Contribution to journalReview Articlepeer-review

26 Downloads (Pure)