Atomic Layer Deposition of Copper Metal Films from Cu(acac)2 and Hydroquinone Reductant

Tripurari Sharan Tripathi, Martin Wilken, Christian Hoppe, Teresa de los Arcos, Guido Grundmeier, Anjana Devi, Maarit Karppinen*