Atomic layer deposition of aluminum fluoride thin films

Miia Mäntymäki (Inventor), Mikko Ritala (Inventor), Markku Leskelä (Inventor)

Research output: Patent

Original languageEnglish
Patent number9394609
Publication statusPublished - 19 Jul 2016
MoE publication typeH1 Granted patent

Cite this