Atomic layer deposition of AlN from AlCl3 using NH3 and Ar/NH3 plasma

Ville Rontu, Perttu Sippola, Mikael Broas, Glenn Ross, Harri Lipsanen, Mervi Paulasto-Kröckel, Sami Franssila

Research output: Contribution to journalArticleScientificpeer-review

24 Citations (Scopus)