Atomic layer deposition and characterization of biocompatible hydroxyapatite thin films

Matti Putkonen, Timo Sajavaara, Paavo Rahkila, Leiting Xu, Sulin Cheng, Lauri Niinistö, Harry J. Whitlow

    Research output: Contribution to journalArticleScientificpeer-review

    72 Citations (Scopus)
    Original languageEnglish
    Pages (from-to)5819-5824
    JournalThin Solid Films
    Volume517
    Publication statusPublished - 2009
    MoE publication typeA1 Journal article-refereed