Anisotropic Nanoindentation Deformation of Ceramic Crystals: 3D-FEM Modeling and Surface Observations

    Research output: Chapter in Book/Report/Conference proceedingConference contributionScientificpeer-review

    Original languageEnglish
    Title of host publicationThe 1st Workshop on Anisotropic Science and Technology, Senri-Chuo, Osaka, Japani, 31.10.-1.11.2004
    EditorsK. Niihara
    Pages102-114
    Publication statusPublished - 2005
    MoE publication typeA4 Article in a conference publication

    Keywords

    • anisotropic pile-up
    • FEM-simulation
    • GaN-crystal
    • nanoindentation
    • sapphire
    • slip
    • twining