Sulphide induced stress corrosion cracking of copper

Activity: Talk or presentation typesConference presentation

Antti Forsström - Speaker

Yuriy Yagodzinskyy - Contributor

Hannu Hänninen - Contributor

Conference presentation
19 Nov 2019

Event (Workshop)

TitleInternational Workshop on Long-term Prediction of Corrosion Damage in Nuclear Waste Systems
Abbrev. TitleLTC
Period19/11/201921/11/2019
Web address (URL)
CityNancy
CountryFrance
Degree of recognitionInternational event