Sulphide induced stress corrosion cracking of copper
Antti Forsström (Speaker)
Yagodzinskyy, Y.
(Contributor)
Hänninen, H.
(Contributor)
Advanced Manufacturing and Materials
Department of Mechanical Engineering
School services, ENG
Activity
:
Talk or presentation types
›
Conference presentation
Description
Conference presentation
Period
19 Nov 2019
Event title
International Workshop on Long-term Prediction of Corrosion Damage in Nuclear Waste Systems
Event type
Workshop
Conference number
7
Location
Nancy, France
Degree of Recognition
International
Keywords
corrosion, spent nuclear fuel disposal